I. Material and Process are Fundamentals
Cast Iron Platform: HT300 integral casting is selected, followed by heat treatment and natural aging for over 3 months, resulting in 30% higher stability than ordinary HT200.
Surface Treatment: Rust-proof treatment extends the lifespan of the precision and prevents deformation caused by corrosion.
Hole Precision: Φ28 hole spacing error ≤0.05mm, ensuring consistent welding.
II. Proper Use
Installation: Support points must be aligned with the main support point to avoid localized stress.
Environment: Keep dry and free from corrosion; temperature controlled between 10-30℃.
Workpieces: Remove workpieces promptly after welding; do not allow workpieces to press against the platform for extended periods.
III. Maintenance is Key
Cleaning: Clean welding slag after each use; anti-spatter liquid reduces adhesion.
Inspection: Measure with a level or autocollimator quarterly; if precision exceeds tolerances, have the manufacturer scrape and re-laminate the workpiece. Maintenance: Check the support points every six months to prevent loosening.
IV. Environmental Control
Temperature and Humidity: Maintain a temperature of 10-30℃ to avoid moisture and corrosion.
Ventilation: Ensure good air circulation in the work area.
Storage: Cover with a dust cover when not in use.